Skip to Main Content
ASM Handbook

Welding, Brazing and Soldering

Edited by
David LeRoy Olson
David LeRoy Olson
Search for other works by this author on:
Thomas A. Siewert
Thomas A. Siewert
Search for other works by this author on:
Stephen Liu
Stephen Liu
Search for other works by this author on:
Glen R. Edwards
Glen R. Edwards
Search for other works by this author on:
ASM International
Volume
6
ISBN electronic:
978-1-62708-173-3
Publication date:
1993
Book Chapter

Procedure Development and Practice Considerations for Solid-State Welding

By
Dan Hauser
Dan Hauser
Edison Welding Institute
Search for other works by this author on:
Published:
1993

Abstract

Diffusion welding involves minimal pressurization, but relatively high temperatures and long periods of time. This article discusses the process variants of diffusion welding: solid-phase and liquid-phase processes. It describes the diffusion welding of carbon and low-alloy steels, high-strength steels, stainless steels, and aluminum-base alloys. The article provides a discussion on dissimilar metal combinations, such as ferrous-to-ferrous combinations, nonferrous-to-nonferrous combinations, ferrous-to-nonferrous combinations, and metal-ceramic joining.

Abstract

Friction welding (FRW) is a solid-state welding process that uses the compressive force of the workpieces that are rotating or moving relative to one another, producing heat and plastically displacing material from the faying surfaces to create a weld. This article reviews practice considerations for the two most common variations: inertia welding and direct-drive friction welding. Direct-drive friction welding differs from inertia welding, primarily in how the energy is delivered to the joint. The article discusses the parameter calculations for inertia welding and direct-drive friction welding. It provides information on friction welding of carbon steels, stainless steels, aluminum-base alloys, and copper-, nickel-, and cobalt-base materials.

You do not currently have access to this content.
Don't already have an account? Register

Dan Hauser, 1993. "Procedure Development and Practice Considerations for Solid-State Welding", Welding, Brazing and Soldering, David LeRoy Olson, Thomas A. Siewert, Stephen Liu, Glen R. Edwards

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal