Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Carbon Fibers

By
Paul J. Walsh
Paul J. Walsh
Zoltek Corporation
Search for other works by this author on:
Published:
2001
Page range:
35 - 40
Publication history
November 01, 2001

Abstract

The earliest commercial use of carbon fibers is often attributed to Thomas Edison's carbonization of cotton and bamboo fibers for incandescent lamp filaments. This article describes the manufacture of PAN-based carbon fibers and pitch-based carbon fibers. It discusses the properties and characteristics of carbon fibers in terms of axial structure, transverse structure, and interfacial bonding. The article discusses the typical applications of carbon fibers, including aerospace and sporting goods. It concludes with a discussion on anticipated developments in carbon fibers.

You do not currently have access to this content.
Don't already have an account? Register

Paul J. Walsh, 2001. "Carbon Fibers", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal