Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Computer Programs

By
Barry J. Berenberg
Barry J. Berenberg
Caldera Composites
Search for other works by this author on:
Published:
2001
Page range:
334 - 343
Publication history
November 01, 2001

Abstract

This article begins with a discussion on criteria for evaluating computer programs for composites structural analysis, including database capabilities, types of engineering calculations supported, interface and operating systems, and technical support. It describes the capabilities of programs, such as CompositePro, ESAComp, and V-Lab that provide a graphical interface, built-in databases, and integrated modules for the different types of analyses. The article reviews the modules of other programs used for composite analysis. The programs include ASCA, CADEC, CoDA, COMPASS, ESDU, LAP, PROMAL, and SACL. The article concludes with information on on-line programs and recourses.

You do not currently have access to this content.
Don't already have an account? Register

Barry J. Berenberg, 2001. "Computer Programs", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal