Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Properties and Performance of Ceramic-Matrix and Carbon-Carbon Composites

By
Cynthia Powell Doğan
Cynthia Powell Doğan
U.S. Department of Energy, Albany Research Center
Search for other works by this author on:
Published:
2001
Page range:
859 - 868
Publication history
November 01, 2001

Abstract

This article discusses the mechanisms for enhancing the reliability of the three types of ceramic-matrix composites, namely, discontinuously reinforced ceramic-matrix composites, continuous fiber ceramic composites, and carbon-carbon composites, along with examples of the mechanical and physical properties. It also presents examples that illustrate the properties of commercially available materials.

You do not currently have access to this content.
Don't already have an account? Register

Cynthia Powell Doğan, 2001. "Properties and Performance of Ceramic-Matrix and Carbon-Carbon Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal