Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Applications of Ceramic-Matrix Composites

By
J.R. Davis
J.R. Davis
Davis & Associates
Search for other works by this author on:
Published:
2001
Page range:
1101 - 1109
Publication history
December 01, 2001

Abstract

The applications of discontinuously reinforced ceramic-matrix composites (CMCs) fall into four major categories, namely, cutting tool inserts; wear-resistant parts; aerospace and military applications; and other industrial applications, including engines and energy-related applications. This article provides examples for these four categories, with emphasis placed on those applications/materials that have achieved commercial viability. The applications for continuous fiber ceramic composites are summarized.

You do not currently have access to this content.
Don't already have an account? Register

J.R. Davis, 2001. "Applications of Ceramic-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal