Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Failure Analysis of Ceramic-Matrix Composites

By
Michael G. Jenkins
Michael G. Jenkins
University of Washington—Seattle
Search for other works by this author on:
Raj N. Singh
Raj N. Singh
University of Cincinnati
Search for other works by this author on:
Published:
2001
Page range:
1000 - 1002
Publication history
November 01, 2001

Abstract

Interpretation of failures of ceramic-matrix composites, and in particular continuous fiber reinforced ceramic-matrix composites is complicated by the complex structure of the composite material. This article describes the failure characteristics and evidence of failure mechanisms of these composites, with illustrations.

You do not currently have access to this content.
Don't already have an account? Register

Michael G. Jenkins, Raj N. Singh, 2001. "Failure Analysis of Ceramic-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal