Civil Infrastructure Applications

By
Vistasp M. Karbhari
Vistasp M. Karbhari
University of California
,
San Diego
Search for other works by this author on:
Published:
2001
Page range:
1091 - 1100
Publication history
November 01, 2001

Abstract

Composites, particularly fiber-reinforced polymer materials, are increasingly being adopted or considered as alternatives to conventional materials for civil infrastructure applications, such as bridges, buildings, waterfront structures, waste treatment facilities, and facilities for transmission and transport of utilities. This article provides information on seismic retrofit applications and discusses the repair and strengthening of components, such as beams, slabs, large-diameter pipes, and bridge decks.

You do not currently have access to this content.
Don't already have an account? Register

Vistasp M. Karbhari, 2001. "Civil Infrastructure Applications", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal