Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Damage Tolerance

By
Mike R. Woodward
Mike R. Woodward
Lockheed Martin Aeronautics Company
Search for other works by this author on:
Rich Stover
Rich Stover
Lockheed Martin Aeronautics Company
Search for other works by this author on:
Published:
2001
Page range:
295 - 301
Publication history
November 01, 2001

Abstract

This article addresses the issue of the implementation of composite damage tolerance requirements as it relates to military aircraft. It presents a brief introduction on the durability impact threat, damage tolerance impact threat, and other damage tolerance damage threats. The article summarizes damage tolerance criteria and durability criteria for military aircraft. It discusses the damage tolerance design philosophy for metallic structures and composite structures of the aircraft. The article describes the implementation of a damage tolerance analysis methodology in terms of mechanics based model, regression algorithm, and semi-empirical analysis methodology.

You do not currently have access to this content.
Don't already have an account? Register

Mike R. Woodward, Rich Stover, 2001. "Damage Tolerance", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal