Vacuum Infusion

By
Arlen Hoebergen
Arlen Hoebergen
Centre of Lightweight Structures TUD-TNO
,
The Netherlands
Search for other works by this author on:
J. Anders Holmberg
J. Anders Holmberg
SICOMP AB
,
Sweden
Search for other works by this author on:
Published:
2001
Page range:
501 - 515
Publication history
November 01, 2001

Abstract

Vacuum infusion is a resin injection technique derived from resin transfer molding. This article discusses the characteristics of the technique and its applications. It presents the theory and background of the technique and provides an illustration of how parts are made. The article provides information on equipment and material used for vacuum infusion. It describes the mechanical properties of components and summarizes the influence of production on the properties. The article concludes with a discussion on design guidelines.

You do not currently have access to this content.
Don't already have an account? Register

Arlen Hoebergen, J. Anders Holmberg, 2001. "Vacuum Infusion", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal