Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Bolted and Bonded Joints

By
L.J. Hart-Smith
L.J. Hart-Smith
The Boeing Company
Search for other works by this author on:
Published:
2001
Page range:
271 - 289
Publication history
November 01, 2001

Abstract

This article provides a discussion on adhesively bonded joints and elastic-plastic mathematical model for an adhesive in shear. It discusses the design rules for thin bonded structures and reviews computer programs for the highly loaded stepped-lap joints. The article describes the two-dimensional effects associated with load redistribution around flaws and with damage tolerance. The elastic-isotropic geometric stress-concentration factors and empirically established correlation factors of mechanically fastened joints are discussed. The article explains the identification of optimal joint proportions for single-row joints. It also discusses the design and analysis of stronger multirow joints, with particular regard to the bearing-bypass interaction.

You do not currently have access to this content.
Don't already have an account? Register

L.J. Hart-Smith, 2001. "Bolted and Bonded Joints", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal