Polyester Resins

By
Tim Pepper
Tim Pepper
Ashland Chemical Company
Search for other works by this author on:
Published:
2001
Page range:
90 - 96
Publication history
November 01, 2001

Abstract

This article provides an overview of the various types of unsaturated polyester resins and low-profile additives. The resins include general-purpose resins, isophthalic resins, bisphenol A fumarate resins, chlorendic resins, and vinyl ester resin. The article describes the mechanical and electrical properties, thermal and oxidative stability, and chemical and ultraviolet (UV) resistance of polyester resins. It concludes with a discussion on the flame-retardant polyester resins.

You do not currently have access to this content.
Don't already have an account? Register

Tim Pepper, 2001. "Polyester Resins", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal