Lamina and Laminate Nonmechanical Testing

By
John Moylan
John Moylan
Delsen Testing Laboratories
Search for other works by this author on:
Published:
2001
Page range:
759 - 765
Publication history
November 01, 2001

Abstract

Characterization of nonmechanical properties is performed in the testing and certification of composite materials. This article focuses on the properties of composites that are commonly investigated. The properties include: per ply thickness; constituent content; density; coefficient of thermal expansion and coefficient of moisture expansion; glass transition temperature; thermal conductivity, diffusivity, and specific heat.

You do not currently have access to this content.
Don't already have an account? Register

John Moylan, 2001. "Lamina and Laminate Nonmechanical Testing", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal