Applications of Carbon-Carbon Composites

By
Kristen M. Kearns
Kristen M. Kearns
Materials and Manufacturing Directorate, Air Force Research Laboratory
Search for other works by this author on:
Published:
2001
Page range:
1067 - 1070
Publication history
November 01, 2001

Abstract

This article presents an overview of the material properties of carbon-carbon composites. It provides information on the applications of carbon-carbon composites in electronic thermal planes, spacecraft thermal doublers, spacecraft thermal shields, spacecraft radiators, and aircraft heat exchangers.

You do not currently have access to this content.
Don't already have an account? Register

Kristen M. Kearns, 2001. "Applications of Carbon-Carbon Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal