Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Introduction to Engineering Mechanics, Analysis, and Design

By
Scott Reeve
Scott Reeve
National Composite Center
Search for other works by this author on:
Published:
2001
Page range:
197 - 198
Publication history
November 01, 2001

Abstract

Composite materials offer amazing opportunities for delivering structures that are optimized to meet design requirements. This article provides a summary of the concepts discussed in the articles under the section “Engineering Mechanics, Analysis, and Design” in ASM Handbook, Volume 21: Composites. The section introduces many of the engineering approaches used in composite industry.

You do not currently have access to this content.
Don't already have an account? Register

Scott Reeve, 2001. "Introduction to Engineering Mechanics, Analysis, and Design", Composites, Daniel B. Miracle, Steven L. Donaldson