Introduction to Manufacturing of Polymer-Matrix Composites

By
B. Tomas Åström
B. Tomas Åström
IFP SICOMP AB
,
Sweden
Search for other works by this author on:
Published:
2001
Page range:
421 - 422
Publication history
November 01, 2001

Abstract

This article explains the key features of manufacturing techniques for polymer composites. It describes the selection of a technically and economically feasible manufacturing technique for a composite design. The article discusses widely accepted and emerging techniques such as open-mold techniques, to manufacture polymer composites.

You do not currently have access to this content.
Don't already have an account? Register

B. Tomas Åström, 2001. "Introduction to Manufacturing of Polymer-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal