Constituent Materials Testing

By
Shari Bugaj
Shari Bugaj
FiberCote Industries, Inc.
Search for other works by this author on:
Published:
2001
Page range:
749 - 758
Publication history
November 01, 2001

Abstract

This article describes the most significant tests to characterize the properties of constituent materials. It discusses the chemical, physical, and mechanical tests for determining the properties of reinforcement fibers and fabrics. The article provides information on some of the basic materials used for thermoset and thermoplastic resin matrices. It reviews the identification of the individual characteristics of thermoset and thermoplastic resin along with the test methods normally used for their determination. The article contains a table that lists properties and tests for uncured and cured thermoset-matrix resins and prepregs.

You do not currently have access to this content.
Don't already have an account? Register

Shari Bugaj, 2001. "Constituent Materials Testing", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal