Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Thermal Analysis

By
George Dallas
George Dallas
TA Instruments
Search for other works by this author on:
Published:
2001
Page range:
973 - 976
Publication history
December 01, 2001

Abstract

This article focuses on various thermal analysis techniques that are used to verify the cure of a polymer composite. The techniques include differential scanning calorimetry (DSC), modulated DSC, thermomechanical analysis, dynamic mechanical analysis, and dielectric analysis. The article also provides an overview of composite failure modes affected by matrix resin and testing approach.

You do not currently have access to this content.
Don't already have an account? Register

George Dallas, 2001. "Thermal Analysis", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal