Quality Assurance of Metal-Matrix Composites

By
William C. Harrigan, Jr.
William C. Harrigan, Jr.
MMC Engineering, Inc.
Search for other works by this author on:
Published:
2001
Page range:
726 - 730
Publication history
November 01, 2001

Abstract

This article describes characterization techniques, mechanical tests, and nondestructive evaluation methods that are commonly used for metal-matrix composites. It also tabulates typical methods of particle size and size distribution measurement, as well as mechanical test specifications for aluminum-matrix composites.

You do not currently have access to this content.
Don't already have an account? Register

William C. Harrigan, Jr., 2001. "Quality Assurance of Metal-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal