Rapid Prototyping

By
David L. Bourell
David L. Bourell
The University of Texas at Austin
Search for other works by this author on:
Joseph J. Beaman, Jr.
Joseph J. Beaman, Jr.
The University of Texas at Austin
Search for other works by this author on:
Donald Klosterman
Donald Klosterman
University of Dayton
Search for other works by this author on:
Ian Gibson
Ian Gibson
University of Hong Kong
Search for other works by this author on:
Amit Bandyopadhyay
Amit Bandyopadhyay
Washington State University
Search for other works by this author on:
Published:
2001
Page range:
383 - 387
Publication history
November 01, 2001

Abstract

This article reviews various rapid prototyping (RP) processes, such as stereolithography, powder sintering, hot melt extrusion, sheet lamination, solid ground curing, and three-dimensional printing. It discusses various material prototypes produced by RP technology. The list of materials includes particulate and fiber-reinforced polymer, ceramic-matrix composites, and metal-matrix composites. The article provides information on freeform-fabrication techniques for composite part lay-up.

You do not currently have access to this content.
Don't already have an account? Register

David L. Bourell, Joseph J. Beaman, Jr., Donald Klosterman, Ian Gibson, Amit Bandyopadhyay, 2001. "Rapid Prototyping", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal