Processing of Metal-Matrix Composites[1]

Published:
2001
Page range:
579 - 588
Publication history
November 01, 2001

Abstract

Metal-matrix composites (MMCs) are a class of materials with a wide variety of structural, wear, and thermal management applications. This article discusses primary processing methods that are used to manufacture discontinuous aluminum MMCs, namely, high-pressure die casting, pressure infiltration casting, liquid metal infiltration, spray deposition, and powder metallurgy methods. It describes the processing of continuous fiber-reinforced aluminum, discontinuously, reinforced titanium, and continuous fiber-reinforced titanium. The article concludes with information on work done to develop magnesium, copper, and superalloy MMCs.

You do not currently have access to this content.
Don't already have an account? Register

2001. "Processing of Metal-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson