Prepreg and Ply Cutting

By
Joe Lautner
Joe Lautner
Gerber Technology Inc.
Search for other works by this author on:
Published:
2001
Page range:
466 - 469
Publication history
November 01, 2001

Abstract

This article reviews the history of prepreg and ply cutting technologies as well as outlines the options available for creating the necessary data and for nesting, cutting, and kitting the plies. It discusses the ways in which these steps influence the workflow for various applications. The characteristics of prepreg and ply cutting methods are presented in a table.

You do not currently have access to this content.
Don't already have an account? Register

Joe Lautner, 2001. "Prepreg and Ply Cutting", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal