Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Failure Analysis Procedures

By
Patricia L. Stumpff
Patricia L. Stumpff
Hartzell Propeller, Inc.
Search for other works by this author on:
Published:
2001
Page range:
953 - 957
Publication history
December 01, 2001

Abstract

This article describes failure analysis procedures for composites and techniques to be used in these analyses. The procedures include a review of available in-service records, materials and processing methods, print requirements, and manufacturing records; visual analysis and nondestructive part evaluation; and verification of materials and processing methods. The article discusses the determination of fiber, matrix, and void volume fractions and verification of ply lay-up and orientation. The review of composites processing parameters; fractography and surface analysis; and mechanical testing and stress analysis are also presented.

You do not currently have access to this content.
Don't already have an account? Register

Patricia L. Stumpff, 2001. "Failure Analysis Procedures", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal