Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Cyanate Ester Resins

By
Susan Robitaille
Susan Robitaille
YLA Inc.
Search for other works by this author on:
Published:
2001
Page range:
126 - 131
Publication history
November 01, 2001

Abstract

Cyanate ester resins are a family of high-temperature thermosetting resins that bridge the gap in thermal performance between engineering epoxy and high-temperature polyimides. This article discusses the chemistry, properties and characteristics of the cyanate ester resins. It describes the processing procedures for the cyanate ester resins and provides information on properties for selected applications, such as space applications, radomes, and printed circuit boards.

You do not currently have access to this content.
Don't already have an account? Register

Susan Robitaille, 2001. "Cyanate Ester Resins", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal