Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Design, Tooling, and Manufacturing Interaction

By
Anthony J. Vizzini
Anthony J. Vizzini
University of Maryland
Search for other works by this author on:
Published:
2001
Page range:
373 - 378
Publication history
November 01, 2001

Abstract

Designing composites for structural performance initially involves meeting a set of desired performance specifications at a minimum cost. This article discusses the factors that are considered in design for manufacturing of polymeric composites. It describes the various aspects of manufacturing, forming process, and post-processing and fabrication for designing the composites.

You do not currently have access to this content.
Don't already have an account? Register

Anthony J. Vizzini, 2001. "Design, Tooling, and Manufacturing Interaction", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal