Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Automotive Applications

By
Nicholas J. Gianaris
Nicholas J. Gianaris
Visteon Corporation
Search for other works by this author on:
Published:
2001
Page range:
1020 - 1028
Publication history
November 01, 2001

Abstract

This article discusses the advantages of polymer matrix composite for automotive application in terms of design drivers, noise, vibration, harshness efficiency, process materials property constraints, safety and reliability, design optimization, structural and appearance requirements, recyclability, and processability. It describes the properties of high-volume composites used in automotive industries. The article provides a discussion on state-of-the-art and developing technologies in automotive field.

You do not currently have access to this content.
Don't already have an account? Register

Nicholas J. Gianaris, 2001. "Automotive Applications", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal