Phenolic Resins

By
Shahid P. Qureshi
Shahid P. Qureshi
Georgia-Pacific Resins, Inc.
Search for other works by this author on:
Published:
2001
Page range:
120 - 125
Publication history
November 01, 2001

Abstract

This article describes the chemistry of phenolic resins and reviews their characteristics and properties for various composites fabrication processes. The fabrication processes include solution/hot-melt process, pultrusion, vacuum infusion, filament winding, sheet molding, and hand lay-up. The article illustrates the manufacturing process of phenolic honeycomb and provides information on the applications of phenolic composites.

You do not currently have access to this content.
Don't already have an account? Register

Shahid P. Qureshi, 2001. "Phenolic Resins", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal