Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Open Molding: Hand Lay-Up and Spray-Up

By
Finn Roger Andresen
Finn Roger Andresen
Reichhold AS
,
Norway
Search for other works by this author on:
Published:
2001
Page range:
450 - 456
Publication history
November 01, 2001

Abstract

Open molding is the method used in the polymer-matrix composites industry to make thermoset composite products. This article discusses the advantages, disadvantages and applications of the open molding. It describes the various process of the open molding, such as hand lay-up process and spray-up process. Workmanship for hand lay-up and spray-up processes is reviewed. The article provides information on the matrix-resin materials used for open molding, including unsaturated polyester resins, epoxy vinyl ester resins, and reinforcements. The article describes the component design and short- and long-term properties of a fiber reinforced composite laminate depending on material selection and workmanship. It also presents basic design guidelines for open molding.

You do not currently have access to this content.
Don't already have an account? Register

Finn Roger Andresen, 2001. "Open Molding: Hand Lay-Up and Spray-Up", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal