Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Introduction to Reinforcing Fibers

By
Frederick T. Wallenberger
Frederick T. Wallenberger
PPG Industries, Inc.
Search for other works by this author on:
Published:
2001
Page range:
23 - 26
Publication history
December 01, 2001

Abstract

Reinforcing fibers are a key component of polymer-matrix composites (PMCs), ceramic-matrix composites (CMCs), and metal-matrix composites (MMCs). This article discusses the mechanical and nonmechanical properties of these composites. It presents an overview of PMC, CMC, and MMC reinforcing fibers. The article describes cost-considered value-in-use of the ultimate-use temperature of selected fibers in three fiber categories: metal fibers or wires, oxide ceramic fibers, and non-oxide ceramic fibers.

You do not currently have access to this content.
Don't already have an account? Register

Frederick T. Wallenberger, 2001. "Introduction to Reinforcing Fibers", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal