Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Tube Rolling

By
Robert J. Basso
Robert J. Basso
Century Design, Inc.
Search for other works by this author on:
Paul A. Roy
Paul A. Roy
Vantage Associates, Inc.
Search for other works by this author on:
Published:
2001
Page range:
565 - 569
Publication history
November 01, 2001

Abstract

This article describes processes and equipment that are used to produce composite tubular parts. The processes include sheeting, pattern cutting, tube rolling, shrink tape debulking, and finishing. The article provides a discussion on materials that are most suitable for tube rolling. These include preimpregnated materials and unidirectional tapes. The article discusses the wrapping techniques, such as convolute and spiral wrapping, of cylindrical and tapered tubes.

You do not currently have access to this content.
Don't already have an account? Register

Robert J. Basso, Paul A. Roy, 2001. "Tube Rolling", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal