Book Chapter

Design Allowables

By
Chris Boshers
Chris Boshers
Composite Materials Characterization, Inc.
Search for other works by this author on:
Published:
2001
Page range:
360 - 365
Publication history
November 01, 2001

Abstract

This article discusses the need for design allowables, development of design allowables, and important factors that affect the selection of allowable. It provides a comparison between lamina and laminate allowables. The article discusses laminate results and specific techniques used in the statistical development of allowable values.

You do not currently have access to this content.
Don't already have an account? Register

Chris Boshers, 2001. "Design Allowables", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal