Recycling and Disposal of Polymer-Matrix Composites

By
John M. Henshaw
John M. Henshaw
The University of Tulsa
Search for other works by this author on:
Published:
2001
Page range:
1006 - 1012
Publication history
November 01, 2001

Abstract

This article begins with a discussion on driving forces for recycling of composites. It reviews the recycling process of thermoset-matrix composites and thermoplastic-matrix composites. The recycling of thermoset-matrix composites includes regrind, chemical, energy recovery, and thermal processes. Thermoplastic-matrix composites are recycled by regrinding, compounding/blending and reprocessing. The article concludes with discussion on the properties of recycled composite fibers.

You do not currently have access to this content.
Don't already have an account? Register

John M. Henshaw, 2001. "Recycling and Disposal of Polymer-Matrix Composites", Composites, Daniel B. Miracle, Steven L. Donaldson