Skip to Main Content
ASM Handbook

Composites

Edited by
Daniel B. Miracle
Daniel B. Miracle
Search for other works by this author on:
Steven L. Donaldson
Steven L. Donaldson
Search for other works by this author on:
ASM International
Volume
21
ISBN electronic:
978-1-62708-195-5
Publication date:
2001
Book Chapter

Design Criteria

By
Greg Kress
Greg Kress
Delta Air Lines
Search for other works by this author on:
Published:
2001
Page range:
353 - 359
Publication history
November 01, 2001

Abstract

This article describes common design criteria and identifies the design considerations that have a significant effect on the end product. The design criteria include cost; size; mechanical properties; repeatability and precision of parts; damage tolerance and durability; and environmental constraints.

You do not currently have access to this content.
Don't already have an account? Register

Greg Kress, 2001. "Design Criteria", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal