Abstract

This article discusses the materials and properties of polymer-matrix composites to characterize each generic material according to its composition and method of manufacture. It contains a table that lists key physical, mechanical, thermal, and electrical properties, and in-service conditions of concern for resin-matrix composites. Axes definitions, symbols, and special property calculations for composite material property tests are reviewed. The article provides an overview of the performance capabilities of selected polymer-matrix composite materials such as thermoplastic-matrix composites and thermoset-matrix composites. The thermoplastic-matrix composites include thermoplastic polyester resins and fiber resin composites; thermoplastic polyamide resins and fiber-resin composites; and thermoplastic polysulfone resins and fiber-resin composites. The thermoset-matrix composites include thermoset polyester resins and fiber resin composites; thermoset phenolic resins and fiber resin composites; thermoset epoxy resins and fiber-resin composites; thermoset polyimide resins and fiber resin composites; and thermoset bismaleimide resins and fiber resin composites.

You do not currently have access to this content.
Don't already have an account? Register

2001. "Properties and Performance", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal