Engineering Mechanics, Analysis, and Design

Published:
2001

Abstract

Composite materials offer amazing opportunities for delivering structures that are optimized to meet design requirements. This article provides a summary of the concepts discussed in the articles under the section “Engineering Mechanics, Analysis, and Design” in ASM Handbook, Volume 21: Composites. The section introduces many of the engineering approaches used in composite industry.

Abstract

A unidirectional fiber composite (UDC) consists of aligned continuous fibers that are embedded in a matrix. This article describes a variety of analytical methods that are used to determine the various physical properties of the UDC. The properties include elasticity, thermal expansion coefficients, moisture swelling coefficients, static and dynamic viscoelastic properties, conductivity, and moisture diffusivity.

You do not currently have access to this content.
Don't already have an account? Register

2001. "Engineering Mechanics, Analysis, and Design", Composites, Daniel B. Miracle, Steven L. Donaldson

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal