Effects of Composition, Processing, and Structure on Properties of Irons and Steels

By
Bruce L. Bramfitt
Bruce L. Bramfitt
Homer Research Laboratories, Bethlehem Steel Corporation
Search for other works by this author on:
Published:
1997
Page range:
357 - 382

Abstract

The properties of irons and steels are linked to the chemical composition, processing path, and resulting microstructure of the material. Processing is a means to develop and control microstructure by hot rolling, quenching, and so forth. This article describes the role of these factors in both theoretical and practical terms, with particular focus on the role of microstructure in various irons. The irons include bainite, pearlite, ferfite, martensite, austenite, ferrite-pearlite, ferrite-cementite, ferrite-martensite, graphite, and cementite. The article discusses the evolution of microstructural change in rail steels, cast iron, and steel sheet. It contains tables that list mechanical properties and compositions of selected steels. The article discusses the basis of material selection of irons and steels.

You do not currently have access to this content.
Don't already have an account? Register

Bruce L. Bramfitt, 1997. "Effects of Composition, Processing, and Structure on Properties of Irons and Steels", Materials Selection and Design, George E. Dieter

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal