Design for Oxidation Resistance

By
James L. Smialek
James L. Smialek
NASA Lewis Research Center
Search for other works by this author on:
;
Charles A. Barrett
Charles A. Barrett
NASA Lewis Research Center
Search for other works by this author on:
;
Jon C. Schaeffer
Jon C. Schaeffer
General Electric Aircraft Engines
Search for other works by this author on:
Published:
1997
Page range:
589 - 602

Abstract

Alloys intended for use in high-temperature environments rely on the formation of a continuous, compact, slow-growing oxide layer for oxidation and hot corrosion resistance. This article focuses on the issues related to high-temperature oxidation of superalloys used in gas turbine engine applications. It discusses general methodologies to evaluate oxidation resistance of materials. The article describes the performance characteristics of superalloys, single-crystal superalloys and other high-temperature materials such as refractory metals and ceramics. It discusses hot corrosion of superalloys and airfoil degradation due to deposits resulting from ingested particles or sand. The article concludes with a discussion on the limitations of testing techniques and life prediction.

You do not currently have access to this content.
Don't already have an account? Register

James L. Smialek, Charles A. Barrett, Jon C. Schaeffer, 1997. "Design for Oxidation Resistance", Materials Selection and Design, George E. Dieter

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal