Manufacturing Processes and Their Selection

By
John A. Schey
John A. Schey
University of Waterloo
Search for other works by this author on:
Published:
1997
Page range:
687 - 704

Abstract

This article explores the possibilities and limitations imposed by manufacturing processes and materials. Detailed design rules for the processes are presented. The article lists the main features of process groups in a tabular form. The physical characteristics and ratings of relative cost and production factors are also tabulated. The process groups include casting; deformation; powder processing; machining; noncutting; joining; ceramic, glass, and polymer processing; and composites manufacturing.

You do not currently have access to this content.
Don't already have an account? Register

John A. Schey, 1997. "Manufacturing Processes and Their Selection", Materials Selection and Design, George E. Dieter

Download citation file:


Close
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal