Skip to Main Content
ASM Handbook

Materials Selection and Design

Edited by
George E. Dieter
George E. Dieter
Search for other works by this author on:
ASM International
Volume
20
ISBN electronic:
978-1-62708-194-8
Publication date:
1997
Book Chapter

Effects of Composition, Processing, and Structure on Properties of Ceramics and Glasses

By
Victor A. Greenhut
Victor A. Greenhut
Rutgersā€”The State University of New Jersey
Search for other works by this author on:
Published:
1997
Page range:
416 - 433

Abstract

This article provides a discussion on various types of glasses, such as traditional glasses, specialty glasses, and glass ceramics. It provides information on glazes and enamels, and reviews the various broad classes of ceramic materials. The broad classes include whitewares, structural clay products, technical ceramics, refractories, structural ceramics, of engineering ceramics, and electronic and magnetic ceramics. General processing variables that can affect structure and compositional homogeneity are discussed. Traditional ceramics that include both oxide and nonoxide ceramics are reviewed. The article presents several examples of engineering ceramics.

You do not currently have access to this content.
Don't already have an account? Register

Victor A. Greenhut, 1997. "Effects of Composition, Processing, and Structure on Properties of Ceramics and Glasses", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal