Design for Fracture Toughness

By
M.P. Blinn
M.P. Blinn
Materials Characterization Laboratory
Search for other works by this author on:
R.A. Williams
R.A. Williams
Materials Characterization Laboratory
Search for other works by this author on:
Published:
1997
Page range:
533 - 544

Abstract

Fracture toughness is the ability of a material to withstand fracture in the presence of cracks. This article focuses on the use of fracture toughness as a parameter for engineering and design purposes. Both linear elastic and elastic-plastic fracture mechanics concepts are reviewed as they relate to fracture toughness and design process. The article explores the use of plane strain fracture toughness, crack-tip opening displacement, and the J-integral as criteria for the design and safe operation of structures and mechanical components. It discusses the variables affecting fracture toughness, including yield strength, loading rate, temperature, and material thickness. A summary of different fatigue and fracture mechanics design philosophies and their relationship with fracture toughness is provided in a table. The article concludes with information on the examples of fracture toughness in design.

You do not currently have access to this content.
Don't already have an account? Register

M.P. Blinn, R.A. Williams, 1997. "Design for Fracture Toughness", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal