Design for Composite Manufacture

By
Anthony J. Vizzini
Anthony J. Vizzini
University of Maryland
Search for other works by this author on:
Published:
1997
Page range:
804 - 810

Abstract

The goal of design is to improve the overall performance of the metal or ceramic matrix rather than to create a material with different response than the base matrix. This article focuses on design for manufacturing of polymeric composites. It discusses the various factors of contact molding, compression-type molding, resin-injection molding, and pultrusion that are considered in designing for composite manufacturing.

You do not currently have access to this content.
Don't already have an account? Register

Anthony J. Vizzini, 1997. "Design for Composite Manufacture", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal