Abstract

This article describes key processing methods and related design, manufacturing, and application considerations for plastic parts. The plastics processing methods include injection molding, extrusion, thermoforming, blow molding, rotational molding, compression molding/transfer molding, composites processing, and casting. The article describes principal features incorporated into the design of plastic parts and concludes with a discussion on materials selection methodology for plastics.

You do not currently have access to this content.
Don't already have an account? Register

Edward A. Muccio, 1997. "Design for Plastics Processing", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal