Skip to Main Content
ASM Handbook

Materials Selection and Design

Edited by
George E. Dieter
George E. Dieter
Search for other works by this author on:
ASM International
Volume
20
ISBN electronic:
978-1-62708-194-8
Publication date:
1997
Book Chapter

Metal Additive Manufacturing—A Review[1][2]

By
William E. Frazier
William E. Frazier
Naval Air Systems Command
Search for other works by this author on:
Published:
1997
Page range:
1 - 9
Publication history
February 03, 2015

Abstract

This article reviews the emerging manufacturing technology that is alternatively called additive manufacturing (AM), direct digital manufacturing, free-form fabrication, three-dimensional (3-D) printing, and so on. It provides a broad contextual overview of metallic AM. The article focuses on the mechanical properties of AM-processed Ti-6Al-4V, IN-625, and IN-718. The development of closed-loop, real-time, sensing, and control systems is essential to the qualification and advancement of AM. This involves the development of coupled process-microstructural models, sensor technology, and control methods and algorithms. AM has the potential to revolutionize the global parts manufacturing and logistics landscape. It enables distributed manufacturing and the productions of parts on demand while offering the potential to reduce cost, energy consumption, and carbon footprint. The article explores the materials science, processes, and business considerations associated with achieving these performance gains. It concludes that a paradigm shift is required to fully exploit AM potential.

You do not currently have access to this content.
Don't already have an account? Register

William E. Frazier, 1997. "Metal Additive Manufacturing—A Review", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal