Abstract

Casting offers the cost advantages over other manufacturing methods for most components. This article reviews the aspects of castings with which designers should be familiar, as well as methods used by foundries to produce high-integrity castings. It discusses the design concepts that designers and foundries can use to obtain maximum performance from cast parts. The article describes the effects of casting discontinuities on properties, including porosity, inclusions, hot tears, metal penetration, and surface defects. A discussion on hot isostatic pressing treatment of castings is provided. The article provides information on solidification simulation and its use in designing castings.

You do not currently have access to this content.
Don't already have an account? Register

Thomas S. Piwonka, 1997. "Design for Casting", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal