Skip to Main Content
ASM Handbook

Materials Selection and Design

Edited by
George E. Dieter
George E. Dieter
Search for other works by this author on:
ASM International
Volume
20
ISBN electronic:
978-1-62708-194-8
Publication date:
1997
Book Chapter

Properties Needed for Electronic and Magnetic Applications

By
Eugene J. Rymaszewski
Eugene J. Rymaszewski
Rensselaer Polytechnic Institute
Search for other works by this author on:
Published:
1997
Page range:
615 - 621

Abstract

This article presents an overview of the electric and magnetic parameters and discusses the significance of these parameters for electronic applications. It describes the components of analog and digital electronic circuits. The article discusses the augmenting technologies: magnetic and special technologies such as electrooptical. It provides information on the special applications of the electric and magnetic parameters.

You do not currently have access to this content.
Don't already have an account? Register

Eugene J. Rymaszewski, 1997. "Properties Needed for Electronic and Magnetic Applications", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal