Sources of Materials Property Data and Information

By
Jack H. Westbrook
Jack H. Westbrook
Brookline Technologies
Search for other works by this author on:
Published:
1997
Page range:
491 - 506

Abstract

This article examines the material property data and information needs at various points in the design, manufacture, and use cycle. It contains a table that lists the various sources of materials data. The article describes the locating media for sources of data, such as suppliers of databases and internet. It discusses the specific types of sources of data, including computer readable media, data centers, and print media. The article reviews methods for evaluation and interpretation of data and discusses the processes of obtaining and reporting test data.

You do not currently have access to this content.
Don't already have an account? Register

Jack H. Westbrook, 1997. "Sources of Materials Property Data and Information", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal