Skip to Main Content
ASM Handbook

Materials Selection and Design

Edited by
George E. Dieter
George E. Dieter
Search for other works by this author on:
ASM International
Volume
20
ISBN electronic:
978-1-62708-194-8
Publication date:
1997
Book Chapter

Fundamental Structure-Property Relationships in Engineering Materials

By
Thomas H. Courtney
Thomas H. Courtney
Michigan Technological University
Search for other works by this author on:
Published:
1997
Page range:
336 - 356

Abstract

This article focuses on the relationships among material properties and material structure. It summarizes the fundamental characteristics of metals, ceramics, and polymers. The article provides information on crystal structure, atomic coordination, and crystalline defects. It discusses the relationships among microstructure and mechanical properties, and the relevance of the properties to design. The article describes the common means for increasing low-temperature strength and presents an example that shows structure-property relationships in nickel-base superalloys for high-temperature applications. The relationships of microstructure with low-temperature fracture, high-temperature fracture, and fatigue failure are also discussed.

You do not currently have access to this content.
Don't already have an account? Register

Thomas H. Courtney, 1997. "Fundamental Structure-Property Relationships in Engineering Materials", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal