Environmental Aspects of Design

By
Shirley T. Fleischmann
Shirley T. Fleischmann
Seymour and Esther Padnos School of Engineering, Grand Valley State University
Search for other works by this author on:
Published:
1997
Page range:
131 - 138

Abstract

This article presents two streams, such as generic concerns and specific concerns, which are suggested by Allenby for environmental aspects of design. It discusses the generic concerns and presents guidelines that provide the structure in which specific techniques can be developed and used. The article provides information on specific methods environmentally responsible for design and specific information that engineers can use. The methods include life cycle assessment, environmental impact assessment, quality function deployment, design for “X”, failure modes and effects analysis, and design for disassembly.

You do not currently have access to this content.
Don't already have an account? Register

Shirley T. Fleischmann, 1997. "Environmental Aspects of Design", Materials Selection and Design, George E. Dieter

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal