Skip to Main Content
ASM Handbook

Metals Process Simulation

Edited by
D.U. Furrer
D.U. Furrer
Search for other works by this author on:
S.L. Semiatin
S.L. Semiatin
Search for other works by this author on:
ASM International
Volume
22B
ISBN electronic:
978-1-62708-197-9
Publication date:
2010
Book Chapter

Texture Measurement and Analysis

By
A.D. Rollett
A.D. Rollett
Carnegie Mellon University
Search for other works by this author on:
Published:
2010
Page range:
92 - 99
Publication history
July 09, 2010

Abstract

This article discusses the central aspect of anisotropy modeling, namely, texture measurement and analysis. It provides an overview of the methods available for characterizing crystallographic preferred orientation, or texture, in polycrystalline materials. These methods include pole figure measurement and electron backscatter diffraction (EBSD). The article describes the process considerations for pole figure measurement, including X-ray diffraction, neutron diffraction, stereographic projection, equal area projection, graphing pole figures, typical textures, and orientation distribution. It also deals with the limitations and challenges associated with the EBSD, and applications of the diffraction.

You do not currently have access to this content.
Don't already have an account? Register

A.D. Rollett, 2010. "Texture Measurement and Analysis", Metals Process Simulation, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal