Modeling and Simulation of Press and Sinter Powder Metallurgy

By
Suk Hwan Chung
Suk Hwan Chung
Hyundai Steel Company
Search for other works by this author on:
Young-Sam Kwon
Young-Sam Kwon
CetaTech, Inc.
Search for other works by this author on:
Seong Jin Park
Seong Jin Park
Pohang University of Science and Technology
Search for other works by this author on:
Randall M. German
Randall M. German
San Diego State University
Search for other works by this author on:
Published:
2010
Page range:
323 - 334
Publication history
February 15, 2010

Abstract

This article presents the governing equations and methodologies to model the press and sinter powder metallurgy, including continuum, micromechanical, multiparticle, and molecular dynamics approaches. It describes the constitutive relation for compaction and sintering. The article discusses the experimental determination of material properties and simulation verification for compaction and sintering. It reviews the use of modeling and simulation of press and sinter powder metallurgy, including gravitational distorting in sintering, compaction optimization, sintering optimization, and coupled press and sinter optimization.

You do not currently have access to this content.
Don't already have an account? Register

Suk Hwan Chung, Young-Sam Kwon, Seong Jin Park, Randall M. German, 2010. "Modeling and Simulation of Press and Sinter Powder Metallurgy", Metals Process Simulation, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal