Simulation of Friction Stir Welding

By
Junde Xu
Junde Xu
Edison Welding Institute Incorporated
Search for other works by this author on:
Jeff J. Bernath
Jeff J. Bernath
Edison Welding Institute Incorporated
Search for other works by this author on:
Published:
2010
Page range:
443 - 451
Publication history
June 30, 2010

Abstract

This article discusses the fundamentals of friction stir welding (FSW) and presents governing equations and an analytical solution for heat transfer. It provides the solutions for structural distortion in FSW. The article describes various techniques that have been adopted to solve the equations and simulate the FSW process. The techniques include modeling without convective heat transfer and modeling with convective heat transfer in a workpiece. The article concludes with information on active research topics in the simulation of FSW.

You do not currently have access to this content.
Don't already have an account? Register

Junde Xu, Jeff J. Bernath, 2010. "Simulation of Friction Stir Welding", Metals Process Simulation, D.U. Furrer, S.L. Semiatin

Download citation file:


×
Close Modal
This Feature Is Available To Subscribers Only

Sign In or Create an Account

Close Modal
Close Modal